In718superalloy相关论文
Effects of Thermally Assisted Warm Laser Shock Processing on the Microstructure and Fatigue Property
The effects of laser shock processing (LSP) and warm laser shock processing (WLSP) on the microstructure of surface hard......
The evolution behavior of the γ″ phase of IN718 superalloy in a temperature/stress coupled field was investigated. Res......
The evolution behavior of the γ″ phase of IN718 superalloy in a temperature/stress coupled field was investigated. Res......